close icon
Leave a message

Please leave a message for more information!

leave a message Leave a message

5059 Aluminum Alloy Plate

Strong Strength, High-Quality Products

5059 Aluminum Alloy Plate Application

1、 5059 has been used as a hull material for small aluminium boats or larger yachts. Its high strength and good corrosion resistance make it an excellent match for yachting.
2、 5059 has been tested for use in vehicle armor.
3、 5059 has been used for cryogenic propellant tanks for experimental reusable rocket vehicles.

5059 Aluminum Alloy Plate description

5059 aluminum alloy is a 5000-series aluminum alloy: the main alloying addition is magnesium, and it is formulated for primary forming into wrought products. 5059 is the Aluminum Association (AA) designation for this material. In European standards, it will be given as EN AW-5059. A95059 is the UNS number. Additionally, the EN chemical designation is AlMg5,5MnZnZr. 5059 aluminum alloy is a wrought alloy type with good corrosion resistance. This alloy cannot be heat treated to gain strength but can be readily welded and retains most of its mechanical strength.
5059 aluminum alloy can be strengthened using strain hardening, or cold mechanical working processes if required. The following datasheet will provide more details about aluminium / aluminum 5059 alloy.


5059 Aluminum Alloy Plate Chemical Composition

Chemical Element

Weight (%)

Aluminum, Al

89.8 - 94

Magnesium, Mg

5-6

Manganese, Mn

0.60-1.2

Iron, Fe

≤ 0.50

Silicon, Si

≤ 0.45

Zinc, Zn

0.40 - 0.90

Chromium, Cr

≤ 0.25

Copper, Cu

≤ 0.25

Titanium, Ti

≤ 0.20

Zirconium, Zr

0.050 - 0.25

Other (each)

≤ 0.050

Other (total)

≤ 0.15


5059 Aluminum Alloy Plate Mechanical properties

–O hardening
Unhardened 5059 has a yield strength of 160 MPa (23 ksi) and ultimate tensile strength of 330 MPa (48 ksi) from −28 to 100 °C (−18 to 212 °F). At cryogenic temperatures it is slightly stronger; above 100 °C (212 °F) its strength is reduced.
Elongation, the strain before material failure, is 24% at room temperature.

–H131 hardening
yield strength of 39.0 ksi (269 MPa), ultimate tensile strength of 52.9 ksi (365 MPa). Produced by Aleris under the AluStar brand. [2]

–H136 hardening
yield strength of 39.0 ksi (269 MPa), ultimate tensile strength of 52.1 ksi (359 MPa). Produced by Aleris under the AluStar brand.

–H321 hardening
H321 strain hardened 5059, with properties measured at 20 °C (68 °F), has yield strength of 270 MPa (39 ksi), ultimate tensile strength of 370 MPa (54 ksi), and elongation of 10%.


hot sale products

aluminum 5052 h32 sheet thicknessaluminum coated sheet
aluminum 6061 data sheetaluminum coated steel sheet
aluminum 6061 t6 data sheetaluminum coil sheet
aluminum 6063 sheetaluminum composite panel sheet
aluminum alloy data sheetaluminum composite sheets